您现在的位置:建筑结构>> 期 刊>> 2014年>> 第11期>>正文内容
榆林城墙改性土加固耐盐性试验研究
陈平1, 汪龙龙1,2, 杨瑜瑞3
摘 要

 

1 西安建筑科技大学土木工程学院, 西安 710055 2 西安公路研究院, 西安7100653 陕西省文化遗产研究院, 西安 710075

摘要]榆林城墙面临消亡的危险,对其加固已迫在眉睫,故提出采用改性土进行加固保护施工方案。为研究加固后城墙的耐久性,在榆林素土中加入少量的掺合料(料姜石、水泥、熟石灰)来改善土体的耐盐性,并对榆林素土和料姜石的化学成分和易溶盐进行分析。试验和实践表明,利用配比为5%水泥、5%熟石灰、10%料姜石、80%黄土的改性土体来夯筑加固城墙,加固后的城墙具有良好的耐久性,这种加固方案能够保持城墙的原貌。

关键词]改性土; 城墙; 料姜石; 加固; 掺合料; 耐盐性

中图分类号:TU472.3       文献标识码:A       文章编号:1002-848X(2014)11-0056-05

Salt resistance experimental research on improved soil reinforcement of Yulin City Wall

Chen Ping1, Wang Longlong12, Yang Yurui3

 (1 Department of Civil Engineering, Xi'an University of Architecture & Technology, Xi'an 710055, China; 2 Xi'an Highway Institute, Xi'an 710065, China; 3 Shaanxi Academy of Cultural Heritage, Xi'an 710075, China)

Abstract: Yulin City Wall faces the danger of disappearing and the reinforcement is immediately needed. The reinforcement protection and construction method of improved soil reinforcement was put forward. In order to research the durability of the reinforced city wall, little amount of mixed stuff, including Liaojiang stone, cement, and hydrated lime, were added into the Yulin soil to improve its salt tolerance property. Chemistry analysis and salt dissolve analysis were proceed on the Yulin soil and Liaojiang stone. The experiment and practice demonstrate that rammed wall with 5% cement, 5% hydrated lime, 10% Liaojiang stone and 80%soil has a well durability, which can maintain the original site of original features.

Keywords: improved soil; city wall; Liaojiang stone; reinforcement; mixed stuff; anti-salt dissolve property

作者简介:陈平,教授,硕士生导师,Emailcping86@hotmail.com

参考文献

1]赵胜杰.高昌故城土遗址病害分析及化学保护研究[D. 西安:西安建筑科技大学,2008.

2GB/T 501231999 土工试验方法标准[S. 北京:中国计划出版社,1999.

3GB/T 1761996 水泥化学分析方法[S. 2008年版.北京:中国计划出版社,2008.

4SY/T 03171997 盐渍土地区建筑规范[S. 北京:中国计划出版社,1997.

5]金德B B.水工建筑物中水泥和混凝土的腐蚀[M.郭成举,译.北京:水利电力出版社,1959.

6]李秀娟. 硫酸盐侵蚀机理及抗硫酸盐侵蚀测试方法的研究[D. 石家庄:河北理工学院,2004.

7READING T J. Combating sulfate attack in Corps of Engineers Concrete ConstructionJ. Concrete Construction1975, 47: 343-366.